Initially I was trying that, but 98% sulfuric acid and 40% hydrogen peroxide needed like 3 days to etch plastic (with like 10 fresh "mixes"). Now I can try that
by BarsMonster 14y ago
Initially I was trying that, but 98% sulfuric acid and 40% hydrogen peroxide needed like 3 days to etch plastic (with like 10 fresh "mixes"). Now I can try that with higher concentrations, would be great if It could lower temperature.
- pbhjpbhj 14y agoHow did you heat it up, microwave?
- BarsMonster 14y agoNo, I use hot-plate and IR thermometer to control temperature.