Excess electrons and holes in silicon spread through spaces on the order of 10nm. Any smaller features will get mixed up. But that's not really what is happeni
by marcosdumay 6y ago
Excess electrons and holes in silicon spread through spaces on the order of 10nm. Any smaller features will get mixed up.
But that's not really what is happening here. The first thing is that those are feature size, not the size of the dopant region. They are like the size of the pixels on a screen, where the transistors get drawn. The second thing is that this limit is for silicon crystals, and top of line chips are now built in 3D with mixed materials, so you can have an entire crystal that is smaller (at least in one dimension) than that limit.