Glass transition temperatures are a little bit misleading, but from personal experience even leaving a PLA print in direct sunlight under even a little tension
by jedimastert 9mo ago
Glass transition temperatures are a little bit misleading, but from personal experience even leaving a PLA print in direct sunlight under even a little tension will cause it to warp in as little as 30 minutes if you aren't careful.