3 ms·
Important point: MCF-7 assays (n = 6) consistently showed that extracts of “barefoot” (no additives) polymers (e.g., LDPE resin P1 in Table 3) were EA free, ev
by userbinator 3y ago
Important point:
MCF-7 assays (n = 6) consistently showed that extracts of “barefoot” (no additives) polymers (e.g., LDPE resin P1 in Table 3) were EA free, even when stressed. (PP-based polymers require antioxidants to prevent severe degradation during their use in manufacturing plastic products.) Furthermore, PE- and PP-based resins containing appropriate additives to produce fit-for-use products could be constructed that remained EA free (n > 100 assays of > 10 resins), even when exposed to common-use stresses.
It's not the plastic itself, it's some of the additives which are problematic.