You don't really need "rosin flux", the idea is to remove oxidation, chloridric acid is what was used for tin soldering, "saturated" with zinc. https://en.wiki
by jaclaz 3y ago
You don't really need "rosin flux", the idea is to remove oxidation, chloridric acid is what was used for tin soldering, "saturated" with zinc.
https://en.wikipedia.org/wiki/Zinc_chloride#As_a_metallurgical_flux https://en.wikipedia.org/wiki/Zinc_chloride#As_a_metallurgic...
Though I have no idea if either can be found locally.
- MisterTea 3y ago> Though I have no idea if either can be found locally. Which is specifically why I mentioned rosin. Though any acid could likely be used so citric acid or something that could work as well.
- jaclaz 3y agoYep, but I don't think that just acid is good enough. Choridric acid + Zinc was traditionally used in tin (but lead isn't so much different) soldering/brazing, particularly of copper and brass because the Zinc had some role in the chemical reaction, AFAIK.