It's the .154" Molex stuff that tends to melt after 20 years spontaneously. Not sure what plating they use bit it turns into a power dissipating resistor after
by gw99 4y ago
It's the .154" Molex stuff that tends to melt after 20 years spontaneously. Not sure what plating they use bit it turns into a power dissipating resistor after a bit which is not good when you're shoving a few amps through it.