I've been messing around with etching for a few months, and I've had quite a lot of luck with a process using a steel plate, a salt-water electrolyte, a power s
by pasabagi 5y ago
I've been messing around with etching for a few months, and I've had quite a lot of luck with a process using a steel plate, a salt-water electrolyte, a power source at 5V or lower, and either a lacquer resist (for WB style relief etching) or a hard wax resist (for traditional etching), then taking a print by putting the plate in a frame, adding a sheet of aluminum gauze, then filling the frame with plaster.
The plaster expands slightly as it sets, so it takes a good print.
The process is not quite as straightforward as the traditional methods, but is much less poisonous, produces no nasty waste products (some clhorine gas, but not much), and doesn't require access to a press.
You can also use it for etching aluminium, which is kind of interesting too. Don't try stainless steel, it doesn't seem to work and you end up with chromium oxides everywhere.
- totetsu 5y agoIs there a name for the plaster technique?
- pasabagi 5y agoI got it from this guy: https://www.youtube.com/watch?v=mDwl0isLpxg https://www.youtube.com/watch?v=mDwl0isLpxg. In my opinion, he makes a bit of a meal out of it: you don't need to take that much care over the frame, but the technique works well. Sometimes if you have a lot of open bite it's tricky to take off the plate without breaking off some of the surface.