3 ms·
Anyone have experience developing 8mm film in caffenol?
by nanna 5y ago
Anyone have experience developing 8mm film in caffenol?
- i_am_proteus 5y agoThe size of the film doesn't matter, only the emulsion. This process is for B&W negative film emulsions. It will work okay with many other film emulsions, but the result will be a B&W negative.
- mmcwilliams 5y agoI've done a fair bit of developing with caffenol and beerol and a combination of the two on moviefilm, mostly 16mm but the process is the same. Volume of the developer is the issue. Works best in a bucket with 2 liters of developer per 400ft of material to prevent exhaustion. I personally like the combination of the traditional caffenol recipe combined with Dagie Brundert's beerol recipe. 1L of water (warm) 100g (20 tsp) washing soda 30g (6 tsp) vitamin C 60g (12 tsp) instant coffee 1L beer On something like Tri-X I'll use a dev time ranging from 15-20 min that I determine after testing. It's a nice balance in contrast between the two developers.
- nanna 5y agoBrilliant. 2 litres developer per 400ft of material seems a bit little though, no? > I personally like the combination of the traditional caffenol recipe combined with Dagie Brundert's beerol recipe. How comes, out of interest?
- mmcwilliams 5y agoFor me beerol doesn't get to the density I'm looking for and caffenol, depending on a few factors, will result in a relatively high-contrast negative. The combined recipe is similar to a stock D-76 or ID-11 in terms of conventional developers. 200ft/L is a conservative estimate and I have been a part of workshops where we developed 1000ft per gallon, so YMMV. Checking my notes it looks like I processed reversal last time I did 4 rolls and so each roll would have been developed twice, essentially.