Just thought of this while reading your post: Could the tin whisker problem be solved by simply reflowing circuit boards every 5-10 years, before they actually
by taneq 7y ago
Just thought of this while reading your post: Could the tin whisker problem be solved by simply reflowing circuit boards every 5-10 years, before they actually short out? I mean, it's labour intensive but for specialized or hobby equipment, might be worth doing.
- marshray 7y agoMost complex boards will have a few parts (like plastic connectors) selectively soldered on after reflow.
- taneq 7y agoTrue. I wonder if you could do something with IR and a mask to selectively heat the bits of the board that’d take it? Then again, later in the slides they talk about simply giving things a scrub with a wire brush to clean off the whiskers. Apparently they don’t regrow after the first few years.
- crististm 7y agoTheoretically - yes. Practically - just imagine the logistics of that.
- johnr2 7y ago> Could the tin whisker problem be solved by simply reflowing circuit boards every 5-10 years Apart from logistics, many components have a hard time surviving the heat of soldering during original manufacture and may fail on subsequent reflowing. Lead free solder typically has a melting point around 35C higher than tin-lead which exacerbates the problem.