> Zhang’s team tested conductivity and structure after heating the silk fibers at 1,050°C (1,922°F) to carbonize the silk protein, and unlike untreated silk, th
by mirimir 10y ago
> Zhang’s team tested conductivity and structure after heating the silk fibers at 1,050°C (1,922°F) to carbonize the silk protein, and unlike untreated silk, the carbon-enhanced silk conducted electricity.
After that much heat, would this silk be useful for making fabric?