2 ms·
I read this whole article hoping to find the part where he tests the tensile strength, impact resistance, stiffness, and dimensional accuracy of the two parts.
by kragen 10y ago
I read this whole article hoping to find the part where he tests the tensile strength, impact resistance, stiffness, and dimensional accuracy of the two parts. It never came. Except for the part where he had a delamination ("split"), which I guess means zero strength for that part of the part.
I've been fairly disappointed with the strength of Prusa-Mendel-printed parts I've made. Even if you don't have complete delaminations, it's easy to get poor layer adhesion, which makes the parts fall apart under the least strain. You can fight that by turning up the temperature and filament feed rate, at the cost of dimensional accuracy (which you can compensate for in theory but I haven't done so successfully, being just an amateur) but the higher heat also weakens the PLA. Maybe this weakening is hydrolysis due to water absorption in the filament; I don't have a way to measure that, except printing the same thing a second time after dehydrating the filament, which I haven't done.
I was surprised to find that 100% infill is not always the strongest option, even holding part geometry constant. Lower infill settings produce a more compliant part, and it can consequently withstand higher impact energies.
I don't think you should hold part geometry constant when changing machines or especially entire fabrication technologies. You should play to the strengths of the machine you have. I know that's contrary to the outlook of 3D printing, but it's true. Things like topology optimization can easily generate forms that are impossible to injection-mold, relatively easy to FDM, and much stronger. If you have the option of 25% infill, you can probably get a stronger part by deploying the plastic you saved as ribs outside the main body. And so on.