I looked it up and the truth is in between. You get "ferritizing" annealing starting at 1300F. Microscopic amounts of that will happen at 500F but nothing sig
by ectoplasm 11y ago
I looked it up and the truth is in between. You get "ferritizing" annealing starting at 1300F. Microscopic amounts of that will happen at 500F but nothing significant. Thank you, now I will stop wasting my time with this piece of folklore...